UHP electrodes graphite late usi sunt in fornace electrico fornacem chalybeam, et praestantem conductivity, excellentem calorem resistentem praebentes, et vires mechanicas, significanter augentes efficientiam et qualitatem productam excoquunt, et essentiales in moderno ferro productiones efficiunt.
The main raw material for manufacturing the body of ultra high power graphite electrodes is imported oil-based needle coke. Processus productionis comprehendit comminuens, protegens, dosing, permixtio, formatio, coquens, alta pressio, impregnatio, coctio secunda, graphitizatio et machinatio. Nipples are made from imported oil-based needle coke using a process of triple impregnation and quadruple baking.
| Parameter | Unitas | Nominal Diameter (mm) | 250~400 | 450~ 550 | 600~ 700 |
| Resistentia | μΩ·m | Electrode | 4.8 ~ 5.8 | 4.5 ~ 5.6 | 4.5 ~ 5.4 |
| Papilla | 3.4 ~ 4.0 | 3.4 ~ 3.8 | 3.0 ~ 3.6 | ||
| inflexio Fortitudo | MPa | Electrode | ≥ 12.0 | ≥ 12.0 | ≥ 10.0 |
| Papilla | ≥ 22.0 | ≥ 22.0 | ≥ 24.0 | ||
| Modulus elasticus | GPa | Electrode | ≤ 13.0 | ≤ 13.0 | ≤ 13.0 |
| Papilla | ≤ 18.0 | ≤ 18.0 | ≤ 20.0 | ||
| mole Density | g/cm³ | Electrode | 1.68 ~ 1.73 | 1.68 ~ 1.72 | 1.68 ~ 1.72 |
| Papilla | 1.78 ~ 1.84 | 1.78 ~ 1.84 | 1.80 ~ 1.86 | ||
| Coefficiens Scelerisque Expansion (CTE) | 10⁻⁶/°C | Electrode | ≤ 1.2 | ≤ 1.2 | ≤ 1.2 |
| Papilla | ≤ 1.0 | ≤ 1.0 | ≤ 1.0 | ||
| Cinis Content | % | ≤ 0.2 | ≤ 0.2 | ≤ 0.2 |
| Nominal Diameter (mm) | Current licita (A) | Current Densitas (A/cm²) |
| 250 | 9000 ~ 14000 | 18 ~ 25 |
| 300 | 15000 ~ 22000 | 20 ~ 30 |
| 350 | 20000 ~ 30000 | 20 ~ 30 |
| 400 | 25000 ~ 40000 | 16 ~ 24 |
| 450 | 32000 ~ 45000 | 19 ~ 27 |
| 500 | 38000 ~ 55000 | 18 ~ 27 |
| 550 | 45000 ~ 65000 | 18 ~ 27 |
| 600 | 52000 ~ 78000 | 18 ~ 27 |
| 650 | 70000 ~ 86000 | 21 ~ 25 |
| 700 | 7MMM ~ 96000 | 18 ~ 24 |