I-electrode ye-graphite ye-300mm ye-RP yimveliso yekhabhoni yomgangatho oqhelekileyo we-power-grade eyenzelwe ngokukodwa ukusetyenziswa kwiindawo ezincinci zombane ze-arc (EAFs), kunye nee-arc furnaces (SAFs) ezisetyenziselwa ukunyibilika kwe-silicon kunye nokuveliswa kwe-phosphorus ephuzi. Esi sisombululo singabizi kakhulu, esamkelwe ngokubanzi sinikezela ukusebenza okuzinzileyo kombane kunye noomatshini kwindawo ephakathi kwe-thermal kunye nomthwalo wombane.
| Ipharamitha | Iyunithi | I-Electrode | Ingono |
| Ukuxhathisa | μΩ·m | 7.5 ~ 8.5 | 5.8 ~ 6.5 |
| Ukugoba Amandla | MPa | ≥ 9 | ≥ 16.0 |
| Imodyuli ye-elastic | GPA | ≤ 9.3 | ≤ 13.0 |
| Ukuxinana ngobuninzi | g/cm³ | 1.55 ~ 1.63 | ≥ 1.74 |
| I-Coefficient of Thermal Expansion (CTE) | 10⁻⁶/°C | ≤ 2.4 | ≤ 2.0 |
| Isiqulatho sothuthu | % | ≤ 0.3 | ≤ 0.3 |
| Ivumelekile ngoku | A | — | 10000 ~ 13000 |
| Ukuxinana kwangoku | A/cm² | — | 14 ~ 18 |
| Okwenyani Ububanzi | mm | Ubukhulu: 307 Imiz: 302 | — |
| Ubude Obubo | mm | 1800 (inokwenziwa ngokwezifiso) | — |
| Ukunyamezela Ubude | mm | ±100 | — |
| Ubude obufutshane boMlawuli | mm | -275 | — |
Ii-electrode ze-RP ziveliswa kwi-petroleum-based calcined coke njengeyona nto iphambili ekrwada, kunye ne-medium-softening-point coal pitch tar esetyenziswa njenge-binder.
Inkqubo yemveliso ibandakanya:
● Ukukhutshwa kwepetroleum coke kwi ~1250°C
● Ukuqulunqa ngokusebenzisa i-high-pressure extrusion okanye ukubumba
● Ukubhaka kokuqala kwi-800-900 ° C ukuzinzisa isakhiwo
● I-Vacuum Pitch Impregnation yokunciphisa i-porosity kunye nokuphucula ukuxhathisa i-oxidation
● Ukubhaka kwakhona ukuqinisa umanyano
● IGraphitizing ukuya kuthi ga kwi-2800 °C kwi-Acheson okanye i-LWG-uhlobo lweziko lokuqhuba kombane kunye nentembeko yesakhiwo.
Umjikelo wonke wemveliso uthatha malunga neentsuku ezingama-45, kuxhomekeke kumthamo wesityalo kunye nokucwangciswa.
● Ii-EAF ezincinci ukuya kweziphakathi kwimveliso ye-carbon kunye ne-alloy steel
● Iziko le-arc eliphantsi kwamanzi kulungiselelwa i-ferrosilicon, isilicon ye-metallurgical-grade, kunye ne-phosphorus etyheli.
● I-Foundry kunye nemisebenzi yokuphosa apho ukusetyenziswa kwe-electrode ephantsi akuyona inkxalabo ephambili
● Iinkqubo ze-Metallurgical ezinemfuno zangoku kunye ne-thermal
● Indawo yokugcina eyomileyo:Gcina kwiindawo ezingenamanzi, ezilawulwa ngubushushu ukuze ugweme i-oxidation yomhlaba kunye nomonakalo wangaphakathi.
● Uluhlu lobushushu:Ubushushu bokugcina obufanelekileyo yi-20–30°C
● Ukupakishwa:Iikhreyiti zomthi ezinobunzima obunogwebu lwangaphakathi kunye nefilimu ekwaziyo ukumelana nokufuma
● Ukuphatha:Sebenzisa izilingi ezingezizo ezentsimbi kunye nezixhobo zokuphakamisa ukunqanda ukonakalisa iziphelo ezinemisonto. Kuphephe ukuqengqeleka i-electrode kwiindawo eziqinileyo ukuthintela ukuqhekeka okanye ukuqhekeka.
● Ukusebenza okungaguquguqukiyo phantsi kwemisebenzi eqhelekileyo ye-EAF
● Ukumelana ne-oxidation ethembekileyo kunye namandla omatshini
● Ukhetho loqoqosho kwimisebenzi eneemfuno zokusebenza eziphakathi
● Iyahambelana neengono ezisemgangathweni we-RP-grade
● Ifuna umsebenzi olawulwayo weziko ngenxa ye-CTE ephezulu