I-electrode ye-graphite engu-300mm RP inikeza isixazululo esingabizi futhi esizinzile sama-EAF amancane naphakathi nendawo, iletha ukuqhutshwa okuthembekile nokumelana ne-oxidation okuhle kakhulu kokukhiqizwa kwe-carbon steel, i-silicon, ne-phosphorus.
I-electrode engu-300mm RP graphite electrode iwumkhiqizo wekhabhoni webanga lamandla ojwayelekile oklanyelwe ukusetshenziswa kuma-arc osayizi omncane kagesi kagesi (EAFs), kanye nama-arc furnaces (ama-SAF) asetshenziswa ekuncibilikiseni i-silicon kanye nokukhiqizwa kwe-phosphorus ephuzi. Lesi sixazululo esingabizi kakhulu, esamukelwe kabanzi siletha ukusebenza okuzinzile kukagesi kanye nemishini ezindaweni ezishisayo ezishisayo nezikagesi.
| Ipharamitha | Iyunithi | I-Electrode | Ingono |
| Ukungazweli | μΩ·m | 7.5 ~ 8.5 | 5.8 ~ 6.5 |
| Ukugoba Amandla | I-MPa | ≥ 9 | ≥ 16.0 |
| I-Elastic Modulus | I-GPa | ≤ 9.3 | ≤ 13.0 |
| Ukuminyana kwenqwaba | g/cm³ | 1.55 ~ 1.63 | ≥ 1.74 |
| I-Coefficient of Thermal Expansion (CTE) | 10⁻⁶/°C | ≤ 2.4 | ≤ 2.0 |
| Okuqukethwe Umlotha | % | ≤ 0.3 | ≤ 0.3 |
| Okuvumelekile Okwamanje | A | — | 10000 ~ 13000 |
| Ukuminyana Kwamanje | A/cm² | — | 14 ~ 18 |
| Ububanzi Bangempela | mm | Ubukhulu: 307 Amaminithi: 302 | — |
| Ubude Bangempela | mm | 1800 (ngezifiso) | — |
| Ukubekezelela Ubude | mm | ±100 | — |
| Ubude Bombusi Omfushane | mm | -275 | — |
Ama-electrode e-RP akhiqizwa kusukela ku-petroleum-based calcined coke njengento yokuqala eluhlaza, ene-medium-softening-point tar pitch yamalahle esetshenziswa njenge-binder.
Inqubo yokukhiqiza ngokuvamile ihlanganisa:
● Ukubalwa kwe-petroleum coke ku-~1250°C
● Ukwakheka ngokusebenzisa i-high-pressure extrusion noma ukubumba
● Ukubhaka Kokuqala ku-800–900°C ukuze kuzinze isakhiwo
● I-Vacuum Pitch Impregnation yokunciphisa i-porosity futhi ithuthukise ukumelana ne-oxidation
● Ukubhaka kabusha ukuze kuqinise ubuhlobo
● Ukwenza i-graphitizing kufika ku-2800°C ezithandweni zohlobo lwe-Acheson noma ze-LWG ukuze kuthuthukiswe ukusebenza kukagesi nobuqotho besakhiwo.
Wonke umjikelezo wokukhiqiza uthatha cishe izinsuku ezingama-45, kuye ngomthamo wezitshalo nokuhlela.
● Ama-EAF amancane kuya kwaphakathi nendawo okukhiqiza i-carbon ne-alloy steel
● Amafurnace e-arc angaphansi kwamanzi okukhiqizwa kwe-ferrosilicon, i-silicon ye-metallurgical-grade, ne-phosphorus ephuzi.
● Imisebenzi yokusungula nokusakaza lapho ukusetshenziswa okuphansi kwama-electrode akuyona into eyinhloko ekhathazayo
● Izinqubo ze-Metallurgical ezinezidingo zamanje nezishisayo ezimaphakathi
● Isitoreji Esomile:Gcina endaweni engenawo umswakama, elawulwa izinga lokushisa ukuze ugweme i-oxidation yendawo kanye nokulimala kwangaphakathi.
● Ibanga Lezinga lokushisa:Izinga lokushisa elilungile lesitoreji ngu-20-30°C
● Ukupakishwa:Amakhreyithi okhuni asindayo anamabhafa amagwebu angaphakathi nefilimu emelana nomswakama
● Ukuphatha:Sebenzisa izihlilingi ezingezona ezensimbi kanye nemishini yokuphakamisa ukuze ugweme ukulimaza iziphetho ezinentambo. Gwema ukugingqa ama-electrode ezindaweni eziqinile ukuze uvimbele ukuqhekeka noma ukuqhekeka.
● Ukusebenza okungaguquguquki ngaphansi kwemisebenzi evamile ye-EAF
● Ukumelana ne-oxidation okuthembekile namandla emishini
● Ukukhetha okunomnotho kwemisebenzi enezidingo zokusebenza okumaphakathi
● Ihambisana nezingono ezisezingeni le-RP-grade
● Idinga ukusebenza kwesithando somlilo esilawulwayo ngenxa ye-CTE yayo ephakeme uma kuqhathaniswa